  1. Have used methonal to thin West System for a number of years now with great results,

    The main reason for thinning the resin is to help reduce the amount of resin used as weight

    can build up very quickly by using this method.

     As a small minus the resin will go off

    faster but you will have plenty of working time. (Mix 50:50)